①低温压力容器受压元件应选用镇静钢。
The low temperature pressure vessel compression element should choose the calm steel.
②低温压力容器受压元件一般要求正火处理,目的细化晶粒,均匀显微组织,降低钢材无塑性转变温度。
The low temperature pressure vessel element general requirements for normalizing treatment to grain refinement and uniform microstructure, reducing the steel nil ductility transition temperature.
③必须做设计温度下低温冲击试验(V)。
Temperature impact test (V) must be done at design temperature.
④钢板δ>20mm,应逐块超声波检测。
The steel plate should be piecewise >20mm, ultrasonic detection.
⑤设计温度在-70到-100区间,目前国内尚无合适材料,可选用奥氏体不锈钢。-100~ -196℃,应选用奥 氏体不锈钢。
The design of temperature in the -70 to -100 range, at present there is no suitable material, can be used for austenitic stainless steel. -196 -100~ C, should be used austenitic stainless steel.
⑥根据《容规》三类容器的主要受压元件应进行材料复检验。
According to the main pressure elements "content regulation" three containers should be material inspection.